• It is a treatment method to prevent further corrosion of reinforcing steel in concrete.
• Bonding layer in concrete repair systems
Standard:
• Compressive strength: ≥ 45Mpa (28 days)
• Flexural tensile strength: ≥ 4 MPa (28 days)
• Adhesion strength: ~1.5Mpa (28 days)
Water dilution ratio: 16-18%
Packaging: 25kg bag